Our products are tried tested, and qualified; adhering to all relevant industry standards including ISO24817 and ASME PCC-2. Below you find a list of case studies of FutureWrap applications in a variety of conditions.  For any enquiries, or further information, please feel free to contact us and we will answer your queries questions as soon as we can.

8 inch sea water return line

An 8-inch sea water return line was suffering from both internal and external corrosion. A temporary repair had been
applied to the line to seal the through…

42 inch hot air line

A 42 inch hot air line was suffering from both external corrosion. Close to a
flange face over time the external corrosion had created a through…

Drilling mud tank

A CSU drilling mud tank, 2.8 meter diameter, which had been out of service for several years was to be re-commissioned. There were several holes…

16 inch crude oil spearator

A 16 inch crude oil separator line was
suffering from internal corrosion. The
measured remaining wall thickness was
3.4 mm. It was estimated that…

Foam tank

A stainless steel foam rectangular tank, 1.2
meter high was suffering from cracking of
the welds. The cause of these defects was
combined manufacturing defects…

14 inch production line

A 14 inch section of duplex pipework
containing gas had mechanical
cracking at one of the welds. An
engineered Futurewrap repair…

36 inch reducer

The weld of a 36 inch cooling water line
was suffering from severe external
corrosion. The corrosion had reduced the
wall thickness such that the weld…

30 inch straight

The weld of a 30 inch straight section of
pipework containing cooling water was
suffering from severe external corrosion.
The corrosion had reduced…

16 inch crude oil spearator

A 16 inch crude oil separator line was
suffering from internal corrosion. The
measured remaining wall thickness was
3.4 mm. It was estimated that…

32 inch glycol still column

A 32 inch line off a glycol still column was
suffering from external corrosion. A
previous composite repair had been
applied and reached the end…

24 inch drilling mud line

A 24 inch drilling mud line was suffering
from external corrosion. It was proposed
to use Futurewrap composite repairs over
4 defects…

6 inch stub

Two 6 inch blanked off stubs at the 6
o’clock position of a gas header vessel on
a FPSO off the west coast of Africa were
suffering…

36 inch produced water caisson (upper section)

Two 6 inch blanked off stubs at the 6
o’clock position of a gas header vessel on
a FPSO off the west coast of Africa were
suffering…

36 inch produced water caisson (lower section)

The lower section of a 36-inch produced
water caisson was suffering from external
corrosion. It was proposed to use a
Futurewrap…